Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastic Armlen® PP 3IM Impact Modified Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Polyplastic Group
Trade Name Armlen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armlen® PP 3IM Impact Modified Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact modified polypropylene composite materialInformation provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1/-2
Flexural Modulus 0.850 GPa
123 ksi
ISO 178
Izod Impact, Notched (ISO) 40.0 kJ/m²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 220 - 230 °C
428 - 446 °F
Mold Temperature 60.0 °C
140 °F
Users viewing this material also viewed the following: