Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastic Armlen® PP MF 20-3IM Impact Modified Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Polyplastic Group
Trade Name Armlen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armlen® PP MF 20-3IM Impact Modified Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact modified polypropylene composite materialInformation provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 2.00 GPa
290 ksi
ISO 527-1
Izod Impact, Notched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ISO 75A
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ISO 75A
Processing Properties Metric English Comments
Melt Temperature 220 - 230 °C
428 - 446 °F
Mold Temperature 60.0 °C
140 °F
Users viewing this material also viewed the following: