Material Notes:
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O) and carbon-carbon (-C-C- bond) comonomer groups are incorporated into its main chain. Therefore the copolymer has superior chemical and thermal stability, compared with acetal homopolymer.Acetal co-polymer is well-balanced in terms of mechanical, chemical and thermal properties, and its superior moldability allows it to be widely employed in various industrial fields.Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ISO 527-1, 2
Elongation at Break 3.0 %
3.0 %
ISO 527-1, 2
Flexural Strength 95.0 MPa
13800 psi
ISO 178
Flexural Modulus 3.00 GPa
435 ksi
ISO 178
Charpy Impact, Notched 0.180 J/cm²
0.857 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C

@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ISO 75-1, 2
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 50 ohm-cm
50 ohm-cm
IEC 60093
Surface Resistance 200 ohm
200 ohm
IEC 60093