Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastics Freqtis® C0711A (PPS/LCP), Molding Compound

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS); Molded
Manufacturer Polyplastics Co.
Trade Name Freqtis®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics Freqtis® C0711A (PPS/LCP), Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Both base resins (PPS and LCP) exhibit excellent heat resistance, dimensional stability and molding processability. Therefore Freqtis® is widely used for surface mounted electronic components. In addition, these compounds have characteristics appropriate for high-frequency device materials on account of their low dielectric losses in high frequency regions.FREQTIS® molding compounds allow dielectric constant control through compounding with a high dielectric constant ceramic developed independently by Otsuka Chemical.p>Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 2.02 g/cc
0.0730 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Flexural Strength 180 MPa
26100 psi
Flexural Strain: 2.2%; ISO 178
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C

@Temperature 20.0 °C
5.56 µin/in-°F

@Temperature 68.0 °F
ISO 11359-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C

@Temperature 20.0 °C
27.8 µin/in-°F

@Temperature 68.0 °F
ISO 11359-2
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Dielectric Constant 7.0

@Frequency 1e+6 Hz
7.0

@Frequency 1e+6 Hz
Volumetric method
Dissipation Factor 0.0020

@Frequency 3.00e+9 Hz
0.0020

@Frequency 3.00e+9 Hz
Perturbation method by cavity resonator
Users viewing this material also viewed the following: