Polyram PB330I8 Nylon 6, 40% Mineral/Glass Filled Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Mineral Filled
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PB330I8 Nylon 6, 40% Mineral/Glass Filled Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 120 MPa

@Thickness 3.17 mm
17400 psi

@Thickness 0.125 in
ASTM D638
Elongation at Break 3.5 %

@Thickness 3.17 mm
3.5 %

@Thickness 0.125 in
ASTM D638
Flexural Strength 250.0 MPa

@Thickness 3.17 mm
36260 psi

@Thickness 0.125 in
ASTM D790
Flexural Modulus 7.52 GPa

@Thickness 3.17 mm
1090 ksi

@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 0.497 J/cm

@Thickness 3.17 mm
0.930 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ASTM D789
Maximum Service Temperature, Air 110 °C
230 °F
Continuous
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in