Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PA320G3 Nylon 6.6 for Injection Molding, 15% Glass Fiber Reinforced, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
15% Glass fiber reinforced flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.2 %
2.2 %
50% RH; ISO 62
Water Absorption at Saturation 7.0 %
7.0 %
ISO 62
Linear Mold Shrinkage 0.0035 - 0.0045 cm/cm
0.0035 - 0.0045 in/in
ISO 2577
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
Tensile Strength, Yield 120 MPa
17400 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Flexural Strength 180 MPa
26100 psi
ISO 178
Flexural Modulus 5.00 GPa
725 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 11357
Maximum Service Temperature, Air 100 °C
212 °F
Continuous use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ISO 75
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 70.0 kV/mm
1780 kV/in
IEC 60250
Users viewing this material also viewed the following: