Polyram PlusTek RA103 Nylon 6.6, Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek RA103 Nylon 6.6, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DIN 53479
Water Absorption 0.95 %
0.95 %
DIN 53495
Linear Mold Shrinkage 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 65.0 MPa
>= 9430 psi
ASTM-D638
Elongation at Break >= 25 %
>= 25 %
ASTM-D638
Flexural Strength >= 95.0 MPa
>= 13800 psi
ASTM D790
Flexural Modulus >= 2.00 GPa
>= 290 ksi
ASTM-D790
Izod Impact, Notched >= 0.800 J/cm

@Temperature 23.0 °C
>= 1.50 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in