Polyram Polytron A30B041 Nylon 66, 30% Long Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron A30B041 Nylon 66, 30% Long Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 170 MPa
24700 psi
ASTM-D638
Elongation at Break 2.5 %
2.5 %
ASTM-D638
Tensile Modulus 9.20 GPa
1330 ksi
ASTM-D790
Flexural Strength 250 MPa
36300 psi
ASTM-D790
Flexural Modulus 9.25 GPa
1340 ksi
ASTM-D790
Izod Impact, Notched 2.10 J/cm

@Temperature 23.0 °C
3.93 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
DSC
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ASTM-D648