Polyram Polytron A30N02 Nylon 66, 30% Long Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name Polytron
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron A30N02 Nylon 66, 30% Long Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 195 MPa
28300 psi
ASTM-D638
Elongation at Break 2.65 %
2.65 %
ASTM-D638
Tensile Modulus 10.65 GPa
1545 ksi
ASTM-D790
Flexural Strength 290 MPa
42100 psi
ASTM-D790
Flexural Modulus 10.7 GPa
1550 ksi
ASTM-D790
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ASTM-D648