Polyram Polytron A40N02 Nylon 66, 40% Long Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron A40N02 Nylon 66, 40% Long Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 230 MPa
33400 psi
ASTM-D638
Elongation at Break 1.9 %
1.9 %
ASTM-D638
Tensile Modulus 13.3 GPa
1930 ksi
ASTM-D790
Flexural Strength 340 MPa
49300 psi
ASTM-D790
Flexural Modulus 11.2 GPa
1620 ksi
ASTM-D790
Izod Impact, Notched 3.00 J/cm

@Temperature 23.0 °C
5.62 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ASTM-D648