Polyram Polytron A50B02 Nylon 66, Chemically Coupled 50% Long Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron A50B02 Nylon 66, Chemically Coupled 50% Long Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 265 MPa
38400 psi
ASTM-D638
Elongation at Break 1.9 %
1.9 %
ASTM-D638
Tensile Modulus 17.2 GPa
2490 ksi
ASTM-D790
Flexural Strength 420 MPa
60900 psi
ASTM-D790
Flexural Modulus 15.5 GPa
2250 ksi
ASTM-D790
Izod Impact, Notched 4.50 J/cm

@Temperature 23.0 °C
8.43 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
487 °F
ASTM-D648