Material Notes:
60% Long fiber glass reinforced natural Nylon 6.6, heat stabilized, for injection molding.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.0 %
1.0 %
50% RH; ISO 62
Water Absorption at Saturation 3.4 %
3.4 %
ISO 62
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 250 MPa
36300 psi
ISO 527
Elongation at Break 1.2 %
1.2 %
ISO 527
Tensile Modulus 23.0 GPa
3340 ksi
ISO 527
Flexural Strength 400 MPa
58000 psi
ISO 178
Flexural Modulus 20.0 GPa
2900 ksi
ISO 178
Izod Impact, Notched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
ISO 180
Charpy Impact Unnotched 15.0 J/cm²
71.4 ft-lb/in²
ISO 179
Charpy Impact, Notched 3.00 J/cm²
14.3 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
487 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in