Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P30N07 Polypropylene, 30% Long Glass Fiber, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A chemically coupled 30% LGF reinforced natural PP, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ISO 527
Elongation at Break 2.6 %
2.6 %
ISO 527
Tensile Modulus 6.00 GPa
870 ksi
ISO 527
Flexural Strength 150 MPa
21800 psi
ISO 178
Flexural Modulus 5.20 GPa
754 ksi
ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
Charpy Impact, Notched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Glow Wire Test 750 °C
1380 °F
GWFI; IEC 60695
Users viewing this material also viewed the following: