Polyram Polytron P40B03 Copolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P40B03 Copolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A CHEMICALLY COUPLED 40% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteristics compared to other grades of Polypropylene long fiber thermoplastics. The room temperature Charpy impact properties are 25 to 30% higher at room temperature and at low temperature (-40 C). Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ASTM-D638
Elongation at Break 2.45 %
2.45 %
ASTM-D638
Tensile Modulus 7.30 GPa
1060 ksi
ASTM-D790
Flexural Strength 155 MPa
22500 psi
ASTM-D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM-D790
Izod Impact, Notched 1.80 J/cm

@Temperature 23.0 °C
3.37 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 151 °C
304 °F
ASTM-D648