Polyram Polytron P60B08-S Polypropylene, 60% Long Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 60% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P60B08-S Polypropylene, 60% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polytron P60B08-S (Single strand) is a chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0045 cm/cm
0.0020 - 0.0045 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 95.0 MPa
13800 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
Tensile Modulus 6.30 GPa
914 ksi
ISO 527
Flexural Strength 135 MPa
19600 psi
ISO 178
Flexural Modulus 6.50 GPa
943 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179
6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179
1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 162 °C
324 °F
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ISO 75
Flame Spread 38 mm/min
1.5 in/min
FMVSS302