Material Notes:
UV stabilized, general purpose, injection molding ASA.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ISO 2577
Melt Flow 25 g/10 min

@Load 10.0 kg,
Temperature 220 °C
25 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Break 60 %
60 %
ISO 527
Tensile Modulus 2.20 GPa
319 ksi
ISO 527
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093