Polyram RamShine PS503 Polystyrene, Flame Retardant

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamShine PS503 Polystyrene, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, high impact polystyrene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM-D638
Elongation at Break 40 %
40 %
ASTM-D638
Tensile Modulus 1.70 GPa
247 ksi
ASTM-D790
Flexural Strength 35.0 MPa
5080 psi
ASTM-D790
Flexural Modulus 1.60 GPa
232 ksi
ASTM-D790
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in