Material Notes:
Impact modified ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Melt Flow 15 g/10 min

@Load 10.0 kg,
Temperature 220 °C
15 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM-D785
Tensile Strength, Yield 47.0 MPa
6820 psi
ASTM-D638
Elongation at Break 25 %
25 %
ASTM-D638
Flexural Strength 74.0 MPa
10700 psi
ASTM-D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM-D790
Izod Impact, Notched 3.00 J/cm

@Temperature 23.0 °C
5.62 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
DIN 53461
Vicat Softening Point 98.0 °C
208 °F
ASTM-D1525
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in