Polyram RamShine PW311G4 SAN, 20% Glass Fiber

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded, Glass Reinforced
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamShine PW311G4 SAN, 20% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Glass fiber reinforced SAN for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption at Saturation 0.10 %
0.10 %
ISO 62
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ISO 2577
Melt Flow 8.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
8.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ISO 527
Tensile Modulus 7.00 GPa
1020 ksi
ISO 527
Flexural Strength 200 MPa
29000 psi
ISO 178
Flexural Modulus 5.20 GPa
754 ksi
ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093