Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamTough PZ126 Polycarbonate, Low Viscosity

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamTough PZ126 Polycarbonate, Low Viscosity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose, low viscosity polycarbonate for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption at Saturation 0.30 %
0.30 %
ISO 62
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ISO 2577
Melt Flow 20 g/10 min

@Load 1.20 kg,
Temperature 300 °C
20 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527
Elongation at Break 85 %
85 %
ISO 527
Tensile Modulus 2.35 GPa
341 ksi
ISO 527
Flexural Strength 100 MPa
14500 psi
ISO 178
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
Izod Impact, Notched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
ISO 75
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
IEC 60093
Dielectric Strength 33.0 kV/mm
838 kV/in
IEC 60250