Material Notes:
Polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 60.0 MPa
>= 8700 psi
ASTM-D638
Elongation at Break >= 80 %
>= 80 %
ASTM-D638
Flexural Strength >= 85.0 MPa
>= 12300 psi
ASTM D790
Flexural Modulus >= 2.10 GPa
>= 305 ksi
ASTM-D790
Izod Impact, Notched >= 5.00 J/cm

@Temperature 23.0 °C
>= 9.37 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) >= 130 °C
>= 266 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) >= 120 °C
>= 248 °F
DIN 53461
Vicat Softening Point 145 °C
293 °F
ASTM-D1525
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in