Precision Polymer Engineering C60M Chloroprene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering C60M Chloroprene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chloroprene Rubber, 56-65 °IRHD. Formulated to meet British Standard BS2752 grade C60.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone and weather.
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
°IRHD; ASTM D1415
63
63
°IRHD, +2 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 13.889 MPa
2014.4 psi
-5% change after 168 hours @ 70°C; ASTM D412
14.62 MPa
2120 psi
ASTM D412
Elongation at Break 280 %
280 %
-12.5% change after 168 hours @ 70°C; ASTM D412
320 %
320 %
ASTM D412
Compression Set 18 %
18 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-30.0 °C
-22.0 °F
Non-brittle after 3 minutes
Flash Point >= 260 °C
>= 500 °F