Precision Polymer Engineering C70G Chloroprene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering C70G Chloroprene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Green Chloroprene Rubber, 72-78 °IRHDApplications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone and weather.
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
°IRHD; ASTM D1415
76
76
°IRHD, +4 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 7.5361 MPa
1093.0 psi
-6.5% change after 168 hours @ 70°C; ASTM D412
8.06 MPa
1170 psi
ASTM D412
Elongation at Break 301.74 %
301.74 %
-6% change after 168 hours @ 70°C; ASTM D412
321 %
321 %
ASTM D412
Compression Set 41 %
41 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flash Point >= 260 °C
>= 500 °F