Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering E70D Ethylene Propylene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering E70D Ethylene Propylene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sulphur cured, Ethylene Propylene Terpolymer, 60-70 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated in accordance with BS2494 Type ‘W’. Water Research Council (WRC) tested to Water Bylaws Scheme ‘Items which have passed full tests of effects on water quality – BS6920’ for use in cold potable water applications.Applications: For joint rings, sealing rings and gaskets used in pipes and fittings associated with potable water systems. WRC approved for cold water applications. WRC Approval No: 0210529
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
°IRHD; ASTM D1415
70
70
°IRHD, +5 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 11.2 MPa
1620 psi
-20% change after 168 hours @ 70°C; ASTM D412
14.0 MPa
2030 psi
ASTM D412
Elongation at Break 304.5 %
304.5 %
-30% change after 168 hours @ 70°C; ASTM D412
435 %
435 %
ASTM D412
Compression Set 14 %
14 %
22 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Flash Point >= 200 °C
>= 392 °F