Material Notes:
Peroxide cured, grey Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage electrical equipment.Applications: Compound designed specially for sealing SF6 gas in electrical distribution equipment, i.e. medium & high voltage switchgear at low temperatures. The specially selected fillers used in this compound impart excellent electrical non-conductive properties to the rubber.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
74
74
°IRHD, +4 change after 70 hours @ 150°C; ASTM D1415
Tensile Strength, Yield 5.00 MPa
725 psi
ASTM D412
Elongation at Break 241 %
241 %
ASTM D412
Compression Set 10.4 %
10.4 %
72 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
-48.0 °C
-54.4 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F