Material Notes:
Nitrile Butadiene Rubber (NBR) 55-65 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5595A Grade 60.Applications: Synthetic rubber resistant to petroleum-based fuels and diester-based lubricants. They are unsuitable for use in contact with phosphate ester hydraulic fluids and have poor ozone resistance.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
60 - 70
60 - 70
°IRHD, -0/+10 change after 168 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 8.10 MPa
1170 psi
-10% change after 168 hours @ 100°C; ASTM D412
9.00 MPa
1310 psi
ASTM D412
Elongation at Break 195 %
195 %
-35% change after 168 hours @ 100°C; ASTM D412
300 %
300 %
ASTM D412
Compression Set 25 %
25 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-30.0 °C
-22.0 °F
Temperature at which stiffness does not exceed 70 Mpa
Flash Point >= 300 °C
>= 572 °F
Users viewing this material also viewed the following: