Precision Polymer Engineering N75L Nitrile Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering N75L Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Ultra-Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000/SAE J200 line call-out: MBF710, B34, F19.Applications: Specifically formulated for use in pure air systems. The low acrylonitrile content of this compound provides excellent resistance to mineral oil, alcohol, paraffin and low-aromatic petrol in sub-zero temperature applications. Not recommended for use with acetone, benzene, chlorinated solvents or high-aromatic petrol. Good water resistance but poor against ozone and weather.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
73
73
°IRHD, +3 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 10.8 MPa
1570 psi
-10% change after 70 hours @ 100°C; ASTM D412
12.0 MPa
1740 psi
ASTM D412
Elongation at Break 214.5 %
214.5 %
-22% change after 70 hours @ 100°C; ASTM D412
275 %
275 %
ASTM D412
Compression Set 15 %
15 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
-56.0 °C
-68.8 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F