Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering Perlast® G70A Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name Perlast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Perlast® G70A Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A black general purpose perfluoroelastomer compound with exceptionally high chemical resistance and excellent steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Do not use any Perlast ® grade with molten alkali metals.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
70
70
°IRHD, 0 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 15.747 MPa
2283.9 psi
-13% change after 72 hours @ 250°C; ASTM D412
18.1 MPa
2630 psi
ASTM D412
Elongation at Break 140 %
140 %
ASTM D412
190.4 %
190.4 %
36% change after 72 hours @ 250°C; ASTM D412
100% Modulus 0.008052 GPa
1.168 ksi
-39% change after 72 hours @ 250°C; ASTM D412
0.0132 GPa
1.91 ksi
ASTM D412
Compression Set 10 %
10 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Flash Point >= 400 °C
>= 752 °F