Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering Perlast® G80X Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name Perlast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Perlast® G80X Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require exposure to temperatures up to 330°C (625°F). Do not use any Perlast ® grade with molten alkali metals.
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
°IRHD; ASTM D1415
79
79
°IRHD, +1 change after 72 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 14.9 MPa
2160 psi
ASTM D412
15.645 MPa
2269.1 psi
5% change after 72 hours @ 200°C; ASTM D412
Elongation at Break 190 %
190 %
ASTM D412
193.8 %
193.8 %
2% change after 72 hours @ 200°C; ASTM D412
100% Modulus 0.00560 GPa
0.812 ksi
ASTM D412
0.00630 GPa
0.914 ksi
12.5% change after 72 hours @ 200°C; ASTM D412
Compression Set 24 %
24 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 330 °C
626 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Flash Point >= 400 °C
>= 752 °F
Copyright © lookpolymers.com All Rights Reserved