Precision Polymer Engineering Q50Y Polyurethane Rubber

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Q50Y Polyurethane Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Yellow/Green Polyurethane Rubber, 50-60 °IRHD. ASTM & ISO designation = AU.Applications: Good abrasion resistance and tensile strength, with fluid compatibility approaching that of NBR. Polyurethane seals provide outstanding performance in hydraulic systems which are prone to abrasive contamination and high shock loads. Good resistance to weathering and ozone but poor against water and high temperature. Good radiation resistance.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
°IRHD; ASTM D1415
66
66
°IRHD, +10 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 13.5 MPa
1960 psi
-25% change after 70 hours @ 100°C; ASTM D412
18.0 MPa
2610 psi
ASTM D412
Elongation at Break 390 %
390 %
-40% change after 70 hours @ 100°C; ASTM D412
650 %
650 %
ASTM D412
Compression Set 28 %
28 %
70 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
-30.0 °C
-22.0 °F
Flash Point >= 204 °C
>= 399 °F