Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering Q90A Polyurethane Rubber

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Q90A Polyurethane Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Peroxide cured, blue Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resistance and tensile strength, with fluid compatibility approaching that of NBR. Polyurethane seals provide outstanding performance in hydraulic systems, which are prone to abrasive contamination and high shock loads. Good resistance to weathering and ozone but poor against water and high temperature.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
°IRHD; ASTM D1415
105
105
°IRHD, +15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 8.00 MPa
1160 psi
-20% change after 70 hours @ 100°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 60.0 %
60.0 %
-40% change after 70 hours @ 100°C; ASTM D412
100 %
100 %
ASTM D412
Compression Set 25 %
25 %
70 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
Non-brittle after 3 minutes
-30.0 °C
-22.0 °F
Flash Point >= 204 °C
>= 399 °F