Material Notes:
Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Excellent steam resistance. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations, Title 21 (CFR21), Section 177.2600. This material is also BgVV Class 15 compliant. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and low temperature flexibility. Used primarily for the manufacture of steam gaskets and autoclave seals. Low physical strength and poor abrasion resistance prevents dynamic sealing.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
62
62
°IRHD, +2 change after 72 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 5.0925 MPa
738.61 psi
-3% change after 72 hours @ 200°C; ASTM D412
5.25 MPa
761 psi
ASTM D412
Elongation at Break 151.3 %
151.3 %
-11% change after 72 hours @ 200°C; ASTM D412
170 %
170 %
ASTM D412
Compression Set 8.0 %
8.0 %
22 hours @ 175°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point >= 300 °C
>= 572 °F