Translucent Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations, Title 21 (CFR21), Section 177.2600. Extraction tested. Compliant to BGA XVA and KTW 1.3.13. ASTM & ISO designation = VMQ.Applications: Excellent mechanical, physical and chemical stability over the temperature range of -40º to +180ºC. Excellent behaviour when sterilised. High transparency grade intended for food contact, pharmaceutical and biomedical applications.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D412
Elongation at Break 520 %
520 %
ASTM D412
Compression Set 40 %
40 %
24 hours @ 175°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Non-brittle after 3 minutes
-40.0 °C
-40.0 °F
Flash Point >= 300 °C
>= 572 °F
Descriptive Properties Value Comments
Extraction Test, 21 CFR 177.2600 pass
Distilled Water
pass
n-Hexane
Users viewing this material also viewed the following: