Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V72H Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V72H Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluoroelastomer Rubber, 65-75 °IRHD. FDA grade. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600.Applications: Excellent oil and heat resistance combine with low compression set performance. Used primarily in food processing and pharmaceutical equipment. Excellent ozone resistance.
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
°IRHD; ASTM D1415
79
79
°IRHD, +7 change after 168 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 9.00 MPa
1310 psi
-25% change after 168 hours @ 250°C; ASTM D412
12.0 MPa
1740 psi
ASTM D412
Elongation at Break 154 %
154 %
-23% change after 168 hours @ 250°C; ASTM D412
200 %
200 %
ASTM D412
Compression Set 35 %
35 %
22 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -25.0 °C
-13.0 °F
ASTM D2137, Non-brittle after 3 minutes
-18.0 °C
-0.400 °F
-17.0 °C
1.40 °F
ASTM D1329, TR10
Flash Point >= 315 °C
>= 599 °F