Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V76E Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V76E Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ETP polymer. This peroxide cured compound is based on a tetrapolymer of Ethylene, Tetrafluoroethylene (TFE) and Perfluoromethylvinylether (PMVE), and a cure site monomer – 70-80 °IRHD.Applications: This compound offers a higher level of fluid resistance than that of fluoroelastomers. It is not totally perfluorinated, so will not exhibit the ultra-low volume swell associated with Perlast® perfluoroelastomers. It is particularly suited to applications which have contact with strong amines, bases, steam and polar solvents. It improves on the chemical resistance of Aflas® and FKM elastomers, while retaining excellent low temperature performance.
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
°IRHD; ASTM D1415
Tensile Strength, Yield 18.4 MPa
2670 psi
ASTM D412
Elongation at Break 180 %
180 %
ASTM D412
Compression Set 20 %
20 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 206 °C
403 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Users viewing this material also viewed the following: