Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V80D Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V80D Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluoroelastomer Rubber, 75-84 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 80.Applications: Mouldings which are required to operate within the approximate temperature range of -20° to +225°C, in contact with air, petroleum, silicone and diester-based liquids. The material is not suitable for use in contact with certain phosphate-ester-based liquids.
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
°IRHD; ASTM D1415
79
79
°IRHD, +1 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 12.75 MPa
1849 psi
-15% change after 72 hours @ 250°C; ASTM D412
15.0 MPa
2180 psi
ASTM D412
Elongation at Break 162 %
162 %
-10% change after 72 hours @ 250°C; ASTM D412
180 %
180 %
ASTM D412
Compression Set 11.5 %
11.5 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 225 °C
437 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Users viewing this material also viewed the following: