Precision Polymer Engineering V95X Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V95X Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluoroelastomer Rubber, 88 - 97 °IRHD. Copolymer of vinylindene fluoride and hexafluoropropylene. Gas-blister resistant fluoroelastomer rubber.Applications: Developed for oil field applications where high pressures are experienced at temperatures in excess of 150°C. The material is a carbon black reinforced, anti-extrusion and gas blister resistant elastomer. It exhibits excellent resistance to compression set.
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
°IRHD; ASTM D1415
93
93
96
96
°IRHD, +5 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 15.2 MPa
2200 psi
-5% change after 72 hours @ 250°C; ASTM D412
16.0 MPa
2320 psi
ASTM D412
Elongation at Break 95.16 %
95.16 %
-20.7% change after 72 hours @ 250°C; ASTM D412
120 %
120 %
ASTM D412
Compression Set 15 %
15 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Descriptive Properties Value Comments
Low Temperature Glass Transition, °C -19