Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V97B Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V97B Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluoroelastomer Rubber, 90-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK914, A1-10, B37, B38, EF31, EO78, Z1. Where Z1 = hardness 90-98. ASTM designation = FKM. ISO designation = FPM.Applications: A hard, anti-extrusion resistant rubber, specially designed for use in high pressure applications. Excellent resistance to oils, fuels and hydraulic fluids at high temperature.
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
°IRHD; ASTM D1415
97
97
°IRHD, +2 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 13.5 MPa
1960 psi
-10% change after 72 hours @ 250°C; ASTM D412
15.0 MPa
2180 psi
ASTM D412
Elongation at Break 90 %
90 %
-10% change after 72 hours @ 250°C; ASTM D412
100 %
100 %
ASTM D412
Compression Set 25 %
25 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 225 °C
437 °F
Minimum Service Temperature, Air -10.0 °C
14.0 °F
Flash Point >= 315 °C
>= 599 °F