Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: Compatible with in-mold coatings, in-mold powder coatings, and many automotive primersExcellent flow and fill in complex molding geometriesMolds well in deep-draw parts as well as in thin-skin moldingsAutomotive Class A surface profile; minimal short and long term wavinessUsed in body panel applications in transportation, recreational, and marine applicationsMarket: Consumer/RecreationalInformation provided by Premix.
Physical Properties Metric English Comments
Specific Gravity 1.78 g/cc
1.78 g/cc
ASTM D792
Linear Mold Shrinkage 0.00068 cm/cm
0.00068 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.5 MPa
9500 psi
ASTM D638
Elongation at Break 1.2 %
1.2 %
ASTM D638
Tensile Modulus 10.3 GPa
1500 ksi
tangent; ASTM D638
Flexural Strength 159 MPa
23000 psi
ASTM D790-1
Flexural Modulus 10.3 GPa
1500 ksi
Tangent; ASTM D790-1
Poissons Ratio 0.30
0.30
ISO 527
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched 11.2 J/cm
21.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
Z-direction; ASTM D696
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Specific Heat Capacity 0.335 J/g-°C
0.0800 BTU/lb-°F
ASTM D1269E
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
ASTM D1269E