Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Premix Thermoplastics PRE-ELEC® PA 1406

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Premix Thermoplastics Inc.
Trade Name PRE-ELEC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PRE-ELEC® PA 1406.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRE-ELEC PA 1406 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon fiber. In addition to a low electrical resistivity PRE-ELEC PA 1406 has an excellent balance of mechanical properties and is easy to injection mould.Typical applications include injection molded technical parts and housings for electronic components and other static sensitive devices (SSD) when high rigidity is needed. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
ISO 868
Tensile Strength, Yield 92.0 MPa
13300 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Modulus of Elasticity 5.00 GPa
725 ksi
ISO 178
Izod Impact, Notched 0.500 J/cm

@Thickness 4.00 mm,
Temperature -20.0 °C
0.937 ft-lb/in

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
5.00 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
9.37 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched 1.25 J/cm

@Thickness 4.00 mm,
Temperature -20.0 °C
2.34 ft-lb/in

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
5.30 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
9.93 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 208 °C
406 °F
ISO 75/Method Bf
Vicat Softening Point 217 °C
423 °F
Rate A; ISO 306/A50
Electrical Properties Metric English Comments
Volume Resistivity <= 1e+05
<= 1e+05
ISO D-257
Surface Resistance <= 1.00e+7 ohm
<= 1.00e+7 ohm
ISO D-257
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C

@Time 7200 - 14400 sec
176 °F

@Time 2.00 - 4.00 hour
Pre-drying in a dehumidifier
Moisture Content <= 0.15 %
<= 0.15 %
When Produced
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Color Black
Injection Speed Moderate
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved