Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Premix Thermoplastics PRE-ELEC® PP 1383

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Premix Thermoplastics Inc.
Trade Name PRE-ELEC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PRE-ELEC® PP 1383.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRE-ELEC PP 1383 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PP 1383 has an excellent balance of mechanical properties and is easy to injection mould. Pre-elec PP 1383 has a very high MFI.Typical applications include injection molded technical parts. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ISO 294-4
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
50 g/10 min

@Load 5.00 kg,
Temperature 230 °C
50 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ISO 868
Hardness, Shore D 65
65
ISO 868
Tensile Strength, Ultimate 28.0 MPa
4060 psi
ISO 527
Elongation at Break 14 %
14 %
ISO 527
Modulus of Elasticity 1.30 GPa
189 ksi
ISO 178
Izod Impact, Notched 0.840 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
1.57 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched NB

@Thickness 4.00 mm,
Temperature 23.0 °C
NB

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ISO 75/Method Bf
Vicat Softening Point 150 °C
302 °F
Rate A; ISO 306/A50
Electrical Properties Metric English Comments
Volume Resistivity <= 100 ohm-cm
<= 100 ohm-cm
ISO D-257
Surface Resistance <= 1000 ohm
<= 1000 ohm
ISO D-257
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 60.0 - 80.0 °C

@Time 7200 - 14400 sec
140 - 176 °F

@Time 2.00 - 4.00 hour
Pre-drying
Moisture Content <= 0.15 %
<= 0.15 %
When Produced
Injection Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Color Black
Injection Speed Moderate
Users viewing this material also viewed the following: