Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Process Technologies Inc
Trade Name Sanifluor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
O-Rings, Gaskets and Seals produced from Sanifluor® 1000 have excellent chemical, heat and steam resistance. They provide superior performance in hot water, steam and virtually all caustics; making them ideal for pharmaceutical, medical, biotechnology, food, beverage and cosmetic manufacturers who use steam or caustic chemicals or a combination of both in their sterilization processes. These very aggressive conditions can be too harsh for commonly used sealing materials such as Silicone, EPDM and FKM. Sanifluor® provides excellent performance in SIP (steam in place), CIP (clean in place) and WFI (water for injection) applications. Sanifluor® 1000 is formulated for use in gaskets and seals where both USP and FDA compliance is required.** It also complies with 3-A Sanitary Standard for multiple-use rubber materials. Sanifluor® 1000 meets the extractive requirements of FDA 21CFR177.2600.Information provided by Process Technologies Inc
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 17.9 MPa
2600 psi
ASTM D1412
Elongation at Break 170 %
170 %
ASTM D1414
50% Modulus 0.00583 GPa
0.845 ksi
ASTM D1414
100% Modulus 0.0118 GPa
1.71 ksi
ASTM D1414
Compression Set 30 %

@Temperature 200 °C,
Time 252000 sec
30 %

@Temperature 392 °F,
Time 70.0 hour
25% Deflection, in Air % of original deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -5.00 °C
23.0 °F
Descriptive Properties Value Comments
Color Black
Compatibility for Chemicals Acetone
Not Recommended
Ammonia
Not Recommended
Hydrochloric Acid
Excellent
Hydrofluoric Acid
Good
Hydrogen Peroxide
Excellent
Isopropyl Alcohol
Excellent
Nitric Acid
Good
Phosphoric Acid
Excellent
Sodium Hydroxide
Excellent
Sodium Hypochlorite
Excellent
Steam to 400ºF (204ºC)
Excellent
Sulfuric Acid
Excellent
Users viewing this material also viewed the following: