Material Notes:
Good reactivity and low viscosity. Outstanding burnout properties with nearly zero ash content.Highly suitable for direct investment casting or dental applications.Information provided by Genistar.
Physical Properties Metric English Comments
Density 1.10 - 1.20 g/cc
0.0397 - 0.0434 lb/in³
Viscosity 350 - 450 cP

@Temperature 23.0 °C
350 - 450 cP

@Temperature 73.4 °F
Ash <= 0.10 %

@Temperature 23.0 °C
<= 0.10 %

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 85
80 - 85
Elongation at Break 1.0 - 5.0 %
1.0 - 5.0 %
Tensile Modulus 1.80 - 2.80 GPa
261 - 406 ksi
Flexural Strength 80.0 - 90.0 MPa
11600 - 13100 psi
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790
Descriptive Properties Value Comments
Appearance Orange