Material Notes:
Superior thermo-mechanical properties.Suitable for the manufacture of parts that require thermal stability, extreme accuracy and quick turnaround. Exceptional for parts that are designed for wind tunnel testing and unique application in rapid tooling or high temperature testing, electrical casings, automotive housingsInformation provided by Genistar.
Physical Properties Metric English Comments
Density 1.50 - 1.60 g/cc
0.0542 - 0.0578 lb/in³
Viscosity 900 - 1300 cP

@Temperature 30.0 °C
900 - 1300 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 92 - 96
92 - 96
Tensile Strength at Break 38.0 - 42.0 MPa
5510 - 6090 psi
ASTM D638
Elongation at Break 0.50 - 1.0 %
0.50 - 1.0 %
ASTM D638
Tensile Modulus 10.0 - 11.0 GPa
1450 - 1600 ksi
ASTM D638
Flexural Strength 145 - 155 MPa
21000 - 22500 psi
ASTM D790
Flexural Modulus 10.0 - 11.0 GPa
1450 - 1600 ksi
ASTM D790
Izod Impact, Notched 0.150 - 0.200 J/cm
0.281 - 0.375 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Appearance Off-white