Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Proto3000 Duraform® AF Selective Laser Sintering (SLS®) Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Nylon
Manufacturer Proto3000
Trade Name Duraform®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 Duraform® AF Selective Laser Sintering (SLS®) Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide (nylon) material with metallic appearance for real-world physical testing and functional use.Features:Metallic appearance with nice surface finishGood powder recycle characteristicsExcellent mechanical stiffnessEasy-to-processDimensionally stable Benefits:Excels in load bearing applications at higher temperaturesBuild prototypes and end-use parts without toolingCreate accurate and repeatable parts as demanded by manufacturers Machinable for demonstration partsImproved isotropic shrinkage due to aluminum fillerApplications: Housings and enclosuresConsumer productsAppropriate for low- to mid-volume rapid manufacturingParts requiring machining or joining with adhesivesComplex production and prototype plastic partsForm, fit or functional prototypesParts requiring stiffnessThermally stressed partsPlastic parts requiring a metallic appearanceInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Bulk Density 0.690 g/cc
0.0249 lb/in³
Density 0.890 g/cc
0.0322 lb/in³
tap
1.42 g/cc
0.0513 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ASTM D2240
Tensile Strength, Ultimate 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Tensile Modulus 3.96 GPa
574 ksi
ASTM D638
Flexural Strength 44.0 MPa
6380 psi
ASTM D790
Flexural Modulus 3.517 GPa
510.1 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.228 J/cm
2.301 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 109 µm/m-°C

@Temperature 35.0 - 172 °C
60.6 µin/in-°F

@Temperature 95.0 - 342 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
356 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 137 °C
279 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+13 ohm-cm
1.60e+13 ohm-cm
ASTM D257
Surface Resistance 6.00e+12 ohm
6.00e+12 ohm
ASTM D257
Dielectric Constant 14.5

@Frequency 1.00e+6 Hz
14.5

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 1.80 kV/mm
45.7 kV/in
ASTM D149
Descriptive Properties Value Comments
Appearance Light grey metallic
Users viewing this material also viewed the following: