Material Notes:
Description: A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts that withstand functional testing. A PC part manufactured on a Fortus 3D Production System is 5-60 percent stronger than a part made on previous FDM systems. It also has superior mechanical properties to ABS and a number of other thermoplastics. When combined with a Fortus system, PC gives you Real Parts™ for conceptual modeling, functional prototyping, manufacturing tools, and end-use-partsAvailable Colors: WhiteInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 68.0 MPa
9860 psi
Type 1, 2"/min; ASTM D638
Elongation at Break 4.8 %
4.8 %
ASTM D638
<= 80 %
<= 80 %
Flexural Elongation; ASTM D790
Tensile Modulus 2.28 GPa
331 ksi
ASTM D638
Flexural Strength 104 MPa
15100 psi
Method 1, 0.05"/min; ASTM D790
Flexural Modulus 2.234 GPa
324.0 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
Method A; ASTM D256
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
Method A; ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 38.0 µm/m-°C
21.1 µin/in-°F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 138 °C

@Thickness 0.125 mm
280 °F

@Thickness 0.00492 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 0.125 mm
261 °F

@Thickness 0.00492 in
ASTM D648
Vicat Softening Point 139 °C
282 °F
ASTM D1525
Glass Transition Temp, Tg 161 °C
322 °F
DAM (SSYS)
Flammability, UL94 V-2

@Thickness 1.10 mm
V-2

@Thickness 0.0433 in
Electrical Properties Metric English Comments
Dielectric Constant 2.96

@Frequency 1.00e+6 Hz
2.96

@Frequency 1.00e+6 Hz
IEC 60250
3.17

@Frequency 60.0 Hz
3.17

@Frequency 60.0 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm