Material Notes:
Description: PC-ISO (polycarbonate-ISO), an industrial thermoplastic, which in its raw state, meets the ISO 10993-1 and USP Class VI classi?cation 1. PC-ISO blends are commonly used in food and drug packaging and medical device manufacturing because of the material’s strength and medical compatibility. When combined with a Fortus 3D Production system, PCISO gives you Real Parts™ that can be used for conceptual modeling, functional prototyping, and end-use parts.Available Colors: White and Translucent NaturalInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 57.0 MPa
8270 psi
Type 1, 2"/min; ASTM D638
Elongation at Break 4.3 %
4.3 %
ASTM D638
4.3 %
4.3 %
Flexural Elongation; ASTM D790
Tensile Modulus 0.998 GPa
145 ksi
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
Method 1, 0.05"/min; ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Notched 0.860 J/cm
1.61 ft-lb/in
Method A; ASTM D256
Izod Impact, Unnotched 0.530 J/cm
0.993 ft-lb/in
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 133 °C

@Thickness 0.125 mm
271 °F

@Thickness 0.00492 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 0.125 mm
261 °F

@Thickness 0.00492 in
ASTM D648
Vicat Softening Point 139 °C
282 °F
ASTM D1525
Glass Transition Temp, Tg 161 °C
322 °F
DAM (SSYS)
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 2.96

@Frequency 1.00e+6 Hz
2.96

@Frequency 1.00e+6 Hz
IEC 60250
3.17

@Frequency 60.0 Hz
3.17

@Frequency 60.0 Hz
IEC 60250