Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Proto3000 PPSF Fused Deposition Modeling Polymer

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer Proto3000
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 PPSF Fused Deposition Modeling Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PPSF/PPSU (polyphenylsulfone) material has the greatest heat and chemical resistance of all Fortus materials - ideal for aerospace, automotive and medical applications. PPSF parts manufactured on Fortus 3D Production Systems are not only mechanically superior, but also dimensionally accurate, to better predict end-product performance. Users can also sterilize PPSF via steam autoclave, EtO sterilization, plasma sterilization, chemical sterilization and radiation. PPSF gives you the ability to manufacture Real Parts™ direct from digital ? les that are ideal for conceptual modeling, functional prototyping, manufacturing tools, and end-use-parts.Available Colors: TanInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
Type 1, 2"/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.068 GPa
299.9 ksi
Type 1, 0.125; ASTM D638
Flexural Strength 110 MPa
16000 psi
Method 1, 0.05"/min; ASTM D790
Flexural Modulus 2.206 GPa
320.0 ksi
ASTM D790
Izod Impact, Notched 0.5873 J/cm
1.100 ft-lb/in
Method A; ASTM D256
Izod Impact, Unnotched 1.655 J/cm
3.100 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C
30.6 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
ASTM D648
Glass Transition Temp, Tg 230 °C
446 °F
DAM (SSYS)
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Constant 3.45

@Frequency 60.0 Hz
3.45

@Frequency 60.0 Hz
IEC 60250
Dielectric Strength 14.6 kV/mm
371 kV/in
IEC 60112
Descriptive Properties Value Comments
Environmental Resistance Antifreeze (Prestone), 50%
Passed, 24 hrs @ 23°C
Antifreeze (Prestone), 50%
Passed, 24 hrs @ 100°C
Gasoline-Unleaded
Passed, 24 hrs @ 23°C
Motor Oil 10W-40
Passed, 24 hrs @ 23°C
Motor Oil 10W-40
Passed, 24 hrs @ 100°C
Power Steering Fluid
Passed, 24 hrs @ 23°C
Power Steering Fluid
Passed, 24 hrs @ 100°C
Transmission Fluid
Passed, 24 hrs @ 23°C
Transmission Fluid
Passed, 24 hrs @ 100°C
Windshield Washer Fluid, 50%
Passed, 24 hrs @ 23°C
Copyright © lookpolymers.com All Rights Reserved