Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer Proto3000
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ULTEM* 9085 is a flame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high strength-to-weight ratio and its V0 rating for FST (flame, smoke, and toxicity). This unique material’s preexisting certifications make it an excellent choice for the commercial transportation industry – especially aerospace, marine and ground vehicles. Combined with a Fortus 3D Production System, ULTEM 9085 allows design and manufacturing engineers to produce fully functional parts that are ideal for advanced functional prototypes or end use without the cost or lead time of traditional tooling.Available Colors: TanInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 71.64 MPa
10390 psi
Type 1, 2"/min; ASTM D638
Elongation at Break 5.9 %
5.9 %
ASTM D790
Tensile Modulus 2.22 GPa
322 ksi
ASTM D638
Flexural Strength 115.1 MPa
16690 psi
Method 1, 0.05"/min; ASTM D790
Flexural Modulus 2.507 GPa
363.6 ksi
ASTM D790
Izod Impact, Notched 1.06 J/cm
1.99 ft-lb/in
Method A; ASTM D256
Izod Impact, Unnotched 6.138 J/cm
11.50 ft-lb/in
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
307 °F
ASTM D648
Glass Transition Temp, Tg 186 °C
367 °F
DAM (SSYS)
Oxygen Index 49 %
49 %
ASTM D2863
Descriptive Properties Value Comments
FAA Flammability <5
FAR 25.853
OSU Peak Heat Release 36 kW/m2
FAR 25.853
OSU Total Heat Release 66 kW.min/m2
FAR 25.853
Vertical Burn 2 seconds
test at (60s), passes at, FAR 25.853