Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek Dense Fused Silica Pre-Cast Shapes

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Dense Fused Silica Pre-Cast Shapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyrocast Dense Fused Silica is an economical product for shapes demanding thermal shock resistance at temperatures. Pyrocast DFS stands up to repeated use in molten metal casting in aluminum, copper, zinc, brass, steel, glass, and aerospace applications. It is durable and resists breakage during handling and cleaning. Components made from Pyrocast Dense Fused Silica resist cracking due to the material's low thermal expansion.ApplicationsSpouts Control pins Mounting seats (inserts) Pre-cast trough tiles Thimbles Wear plates Trough dams AdvantagesResistant to thermal shock Superior strength Low thermal expansion Economically priced Resistant to surface corrosion Able to rapidly cycle Computer controlled firing Superior material consistency Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.76 - 1.95 g/cc
0.0636 - 0.0704 lb/in³
Open Porosity 8.0 - 10 %
8.0 - 10 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0170 - 0.0200 GPa
2.47 - 2.90 ksi
Compressive Strength 48.0 - 51.0 MPa
6960 - 7400 psi
Thermal Properties Metric English Comments
CTE, linear 0.500 - 0.700 µm/m-°C

@Temperature 20.0 °C
0.278 - 0.389 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.800 W/m-K

@Temperature 13.0 °C
5.55 BTU-in/hr-ft²-°F

@Temperature 55.4 °F
Maximum Service Temperature, Air 1090 °C
1990 °F
Sustained
1650 °C
3000 °F
Peak
Component Elements Properties Metric English Comments
Al2O3 0.30 %
0.30 %
CaO 0.020 %
0.020 %
Fe2O3 0.020 %
0.020 %
MgO 0.020 %
0.020 %
SiO2 99.6 %
99.6 %
TiO2 0.010 %
0.010 %
Users viewing this material also viewed the following: